Japan imported Kaka clean agent
Update time:2022/01/20
Japan imported Kaka clean agent

Japan imported Kaka clean agent

 K series of slag agent KAGALITE Co., Ltd. of Japan imported high-performance casting slag dedicated slag products

 Product features and features

 1, adding less, slagging ability, easy crusting, removal;

2, the slag is brittle, non-stick package; lining lining to improve the service life;

3, the proportion of light, large expansion coefficient, covering insulation performance, the treatment of molten metal temperature drop is small;

4, the effective coverage of the metal surface to reduce the smelting of alloying elements oxidation;

5, does not change the metal composition, does not pollute the metal liquid;

6, the use of smoke-free clean, clean workshop production environment.

product manual

 1, electric smelting, when the metal liquefied, the liquid metal surface in a small amount of slag agent initially slag, and then sprinkle a thin layer covered in metal

 Liquid surface from the role of thermal insulation and slag, baked slag before baking.

 2, molten steel water before the bottom of the ladle can be sprinkled a little slag agent. However, before the cast iron water, do not put the bottom of the ladle slag agent, so as not to

 Affect the effect of the ball inoculation.

3, in the ladle hot metal surface sprinkle a little slag agent, after slag, and then sprinkle a little cover can be cast.

 4, the total amount of about 0.1-0.2% of the weight of molten metal.

 Product Specifications:

Product name

Particle size

Granularity

H2O

NET(kg)

Casting applications

 K-0

 4.750-2.360

 4-7.5

 50% or less

 20kg/bag

 Stainless steel, carbon steel

 K-1

 2.360-1.180

 7.5-14

 1% or less

 20kg/bag

 Stainless steel, carbon steel

 K-2

 1.400-425

 12-36

 0.5% or less

 20kg/bag

 Stainless steel, carbon steel

 K-3M

 600-300

 26-50


 20kg/bag

 Cast iron, ductile iron

 K-34

 500-90

 30-200


 20kg/bag

 Cast iron, ductile iron

 K-4M

 300-63

 50-235


 20kg/bag

 Cast iron, ductile iron


Proportion

Unit volume (packing)0.5-0.9kg/L

Refractoriness

SK02a (1060℃)

Thermal Conductivity

0.280-0.341 kca1/mh℃

Sound absorption rate

60%

PH

7

Water absorption

15-28%

Oil absorption

10-24%

Freezing test

-20 ℃ environment for 24 hours, no change

Porosity experiment

48.6%(JIS R2641),42.9%(JIS R2215)

Chemical resistance

Natural glass chemical resistance, chemical properties are stable

 Chemical composition (standard): 

SIO2

AL2O3

Fe2O3

CaO

MgO

K2O

Na2O

IG

74.2%

12.9%

1.05%

0.80%

0.11%

4.54%

3.19%

3.3%